Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® K TC8SCE Thermoplastic Elastomer, high scratch resistance

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TC8SCE Thermoplastic Elastomer, high scratch resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The SCR Series is recommended for applications requiring a high degree of scratch resistance. The series is characterized, among other things, by a pleasant feel. Typical applications: Car matsFunction and design elementsHandles (tools, toolboxes, ski poles) Soft touch surface (thumb wheels, push buttons, switches)Material advantages: Adhesion to PPEasy coloring (compounds in natural colors) Excellent abrasion resistanceExcellent mechanical propertiesExcellent scratch resistancePleasant surface feel (Soft touch)Processing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
DIN ISO 7619
Tensile Strength 11.5 MPa
1670 psi
DIN 53504/ISO 37
Elongation at Break 550 %
550 %
DIN 53504/ISO 37
Tear Strength 22.0 kN/m
126 pli
DIN ISO 34-1
Compression Set 36 %

@Temperature 25.0 °C,
Time 259000 sec
36 %

@Temperature 77.0 °F,
Time 72.0 hour
DIN ISO 815
80 %

@Temperature 70.0 °C,
Time 86400 sec
80 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
86 %

@Temperature 100 °C,
Time 86400 sec
86 %

@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 200 °C
392 °F
Front Barrel Temperature 220 °C
428 °F
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Natural
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C
Scratch resistance 0.85
acc. PV 3952 10N
Copyright © lookpolymers.com All Rights Reserved