Material Notes:
The UV/AP Series is recommended for applications requiring high UV resistance. It is particularly suited for automotive exterior components. The compounds comply with GM standard GMW 16233. Typical applications: Roof rimsWater deflectorsWindow encapsulationsMaterial advantages: Adhesion to PPEasy flowingExcellent mechanical propertiesExcellent UV- and weather resistanceProcessing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
DIN ISO 7619
Tensile Strength 5.20 MPa
754 psi
DIN 53504/ISO 37
Elongation at Break 600 %
600 %
DIN 53504/ISO 37
Tear Strength 20.0 kN/m
114 pli
DIN ISO 34-1
Compression Set 21 %

@Temperature 25.0 °C,
Time 259000 sec
21 %

@Temperature 77.0 °F,
Time 72.0 hour
DIN ISO 815
52 %

@Temperature 70.0 °C,
Time 86400 sec
52 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
72 %

@Temperature 100 °C,
Time 86400 sec
72 %

@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 200 °C
392 °F
Front Barrel Temperature 220 °C
428 °F
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Black
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C
Copyright © lookpolymers.com All Rights Reserved