Kraiburg TPE THERMOLAST® K TA7FAA Food Grade TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TA7FAA Food Grade TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compound easy printable, paintable, glueable without pretreatmentColorable in any shadeSubstitution for PVC and silicone rubberTypical Applications: ToysBaby productsPromotion articlesMaterial Advantages: BgVV/FDA and EN 71/3 compliantGlueable with acrylate glueExcellent tensile strengthPrintable, decorable, and paintable without pretreatmentAdhesion to PSExcellent flow characteristicsProcessing: Like polyolefinsApply back pressure for high wall thicknessInformation provided by Kraiburg TPE.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
DIN 53505
Tensile Strength at Break 14.8 MPa
2150 psi
DIN 53504
Elongation at Break 600 %
600 %
DIN 53504
Tear Strength 30.0 kN/m
171 pli
DIN 53515
Processing Properties Metric English Comments
Processing Temperature 160 - 200 °C
320 - 392 °F
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Descriptive Properties Value Comments
Color Natural