Category | Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE |
Manufacturer | Kraiburg TPE |
Trade Name | THERMOLAST® A |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Kraiburg TPE THERMOLAST® A TA5AOZ Thermoplastic Elastomer, Outdoor application with adhesion to PC, PC/ABS and optimized scratch resistance.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 g/cc | 0.0415 lb/in³ | DIN EN ISO 1183-1 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 47 | 47 | DIN ISO 7619 |
Tensile Strength | 3.00 MPa | 435 psi | DIN 53504/ISO 37 |
Elongation at Break | 600 % | 600 % | DIN 53504/ISO 37 |
Tear Strength | 13.0 kN/m | 74.2 pli | DIN ISO 34-1 |
Peel Strength | 1.50 kN/m | 8.56 pli | ABS; D41 1916 |
4.00 kN/m | 22.8 pli | PC/ABS; D41 1916 | |
5.00 kN/m | 28.5 pli | PC; D41 1916 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 180 °C | 356 °F | |
Middle Barrel Temperature | 210 °C | 410 °F | |
Front Barrel Temperature | 240 °C | 464 °F | |
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Drying Temperature | 60.0 - 80.0 °C @Time 7200 - 14400 sec |
140 - 176 °F @Time 2.00 - 4.00 hour |
|
Injection Pressure | 20.0 - 100 MPa | 2900 - 14500 psi | |
Back Pressure | 1.97 - 4.90 MPa | 285 - 710 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Black | |
Hotrunner | 200-250°C | The runner should be empty after a maximum of 2 - 3 shots. |
Max Cylinder Temperature | 250°C |