Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® A TA4AOZ Thermoplastic Elastomer, Outdoor application with adhesion to PC, PC/ABS and optimized scratch resistance

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® A
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® A TA4AOZ Thermoplastic Elastomer, Outdoor application with adhesion to PC, PC/ABS and optimized scratch resistance.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The UV/AD1 Series is recommended for applications requiring a high UV resistance and adhesion to polar thermoplastics such as PC, ABS, PC/ABS. It is particularly appropriate for automotive exterior components. Typical applications: Handles (hand tools and power tools etc.)Seals for windows and doorsMaterial advantages: Easy flowingExcellent adhesionPerfect surface finishUV resistanceProcessing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
DIN ISO 7619
Tensile Strength 2.00 MPa
290 psi
DIN 53504/ISO 37
Elongation at Break 500 %
500 %
DIN 53504/ISO 37
Tear Strength 8.50 kN/m
48.5 pli
DIN ISO 34-1
Peel Strength 0.500 kN/m
2.85 pli
ABS; D41 1916
3.00 kN/m
17.1 pli
PC; D41 1916
3.00 kN/m
17.1 pli
PC/ABS; D41 1916
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 240 °C
464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Black
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C