Material Notes:
The AD/PAX/MR Series is recommended for two-component-seals in electronic applications and soft touch grips and handles of machine tools. The material provides an excellent resistance to skin oils, sunscreen, olive oil and acetone, accompanied by outstanding adhesion properties to semi-aromatic polyamides and polyarylamides such as PA 12, PA 6 und PA 6.6. The series is available in natural and black colors. Typical applications: Attenuators for electronic housingsConnectorsHandles (Power tool) SealsSeals for computer and laptop screensSeals for housingsMaterial advantages: Easy coloring (compounds in natural colors) Excellent adhesion to semi-aromatic Polyamides, Polyarylamides, Polyamides like PA 12, PA 6 and PA 6.61Excellent mechanical propertiesResistance against skin oils, sunscreens, olive oil and acetoneProcessing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
DIN ISO 7619
Tensile Strength 6.50 MPa
943 psi
DIN 53504/ISO 37
Elongation at Break 850 %
850 %
DIN 53504/ISO 37
Tear Strength 29.5 kN/m
168 pli
DIN ISO 34-1
Peel Strength 7.00 kN/m
39.9 pli
PARA; D41 1916
30.0 kN/m
171 pli
Haftung (PAX); D41 1916
Compression Set 30 %

@Temperature 25.0 °C,
Time 259000 sec
30 %

@Temperature 77.0 °F,
Time 72.0 hour
DIN ISO 815
60 %

@Temperature 70.0 °C,
Time 86400 sec
60 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
73 %

@Temperature 100 °C,
Time 86400 sec
73 %

@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 240 °C
464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
A temperature exceeding 80 °C (175 °F) should be avoided
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Natural
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C