Material Notes:
The VS/MR/AD1 Series is recommended for applications in the consumer electronics section. The series features an exceptionally silky and velvety surface, accompanied by an outstanding resistance to skin oil, sun cream and olive oil. The compounds convince due to their excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. Typical applications: Ear phonesGame consolesHandles and grips for consumer applicationsRemote controlsSealsMaterial advantages: Easy coloring (compounds in natural colors) Excellent color stabilityGood weathering resistanceInsert molding possiblePleasant surface feel (Soft touch)Resistance against skin oil, sunscreens and olive oilSmooth and silky surfaceProcessing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
DIN ISO 7619
Tensile Strength 8.50 MPa
1230 psi
DIN 53504/ISO 37
Elongation at Break 800 %
800 %
DIN 53504/ISO 37
Tear Strength 23.0 kN/m
131 pli
DIN ISO 34-1
Peel Strength 23.0 kN/m
131 pli
PC; D41 1916
25.0 kN/m
143 pli
ABS; D41 1916
Processing Properties Metric English Comments
Rear Barrel Temperature 160 °C
320 °F
Middle Barrel Temperature 180 °C
356 °F
Front Barrel Temperature 200 °C
392 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
A temperature exceeding 80 °C (175 °F) should be avoided
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments