Kotec Carbotex K-30F5 Polycarbonate, Wear Resistant

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Kotec Corp
Trade Name Carbotex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kotec Carbotex K-30F5 Polycarbonate, Wear Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Wear resistance, TranslucentApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation provided by Kotec Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C,
Time 86400 sec
0.20 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D995
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm

@Temperature 23.0 °C
2.81 ft-lb/in

@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 132 °C
270 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.00080

@Frequency 1.00e+6 Hz
0.00080

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Descriptive Properties Value Comments
Light Transmittance Translucent
3.0mm, ASTM D1003