Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High heat stability, outstanding abrasion resistance, excellent electrical properties, good surface gloss, low water absorption, excellent chemical resistance, good processabilityInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.050 %
0.050 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
DIN 53505; ASTM D785
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Elongation at Break 7.0 %
7.0 %
DIN 53455; ASTM D638
Flexural Yield Strength 216 MPa
31300 psi
DIN 53455; ASTM D790
Flexural Modulus 8.83 GPa
1280 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 224 °C
435 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
DIN 53461; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 27.0 kV/mm
686 kV/in
ASTM D149/DIN 53481
Arc Resistance 110 sec
110 sec
ASTM D495
Users viewing this material also viewed the following: