Kolon Kopa® KN173HI Nylon 6 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Kolon
Trade Name Kopa®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon Kopa® KN173HI Nylon 6 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent chemical resistance, Wide usage temperature, Good impact absorbing characteristics. Information provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
DIN 53479; ASTM D792
Water Absorption 1.5 %
1.5 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
0.013 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
DIN 53505; ASTM D785
Tensile Strength, Ultimate 64.0 MPa
9280 psi
DIN 53455; ASTM D638
Elongation at Break 200 %
200 %
DIN 53455; ASTM D638
Flexural Yield Strength 98.0 MPa
14200 psi
DIN 53452; ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.980 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149/DIN 53481
Arc Resistance 125 sec
125 sec
ASTM D495