Material Notes:
Hybrid, dimensionally stableApplications Timing belt coversInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.40 %
0.40 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength 116 MPa
16800 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.884 GPa
853.4 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 233 °C
451 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.4
3.4
ASTM D150
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149
Arc Resistance 135 sec
135 sec
ASTM D495