Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Kolon
Trade Name Kopa®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.60 %
0.60 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
0.013 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 80.0 MPa
11600 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 132 MPa
19100 psi
ASTM D790
Flexural Modulus 3.138 GPa
455.1 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.4
3.4
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Arc Resistance 125 sec
125 sec
ASTM D495