Kleerdex Kydex® GND Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® GND Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive fire-rated sheetApplications: Electronic equipment where protection against electro-static damage is essential, conductive floor mats, IC containers like trays, storage bins, boxes, chip carriers, tray divider, internal electronic equipment or components requiring a UL 94 V-0 ratingFeatures: Unlike other conductive sheet grades, Kydex GND retains its conductance even after forming. For deep or hard to form parts, Kydex GND outperforms the competitive conductive sheet in thermoformability. It is very resistant to a broad range of chemicals, particularly to acids and bases. Kydex GND is very rigid. It meets the requirements of UL Standard 94 V-0.Fabrication: Kydex GND is easy to form and retains its conductive properties after forming. Excellent forming properties result in uniform wall thickness and crisp detail, plus easy machining and fabricating using conventional methods and equipment.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Ultimate 33.0 MPa
4790 psi
ASTM D638
Elongation at Break 106 %
106 %
Modulus of Elasticity 1.868 GPa
270.9 ksi
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Izod Impact, Notched 1.07 - 1.60 J/cm

@Temperature 23.0 °C
2.00 - 3.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05
1e+05
ASTM D257