Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may occur. Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrests.Features: Kydex 1900 has improved heat distortion temperature for higher in-service temperatures. It meets FAR 25.853(a) for vertical burn and is available in a wide range of textures, color, thickness, and sheet sizes. Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 100 %
100 %
Modulus of Elasticity 2.517 GPa
365.1 ksi
Flexural Yield Strength 69.0 MPa
10000 psi
ASTM D790
Izod Impact, Notched 6.00 - 9.00 J/cm

@Temperature 23.0 °C
11.2 - 16.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature