Material Notes:
High rigidity sheet for ceiling panelsApplications: Ceiling panels in clean rooms, computer rooms, laboratories, food, dairy, and pharmaceutical plants, and other environments where a high degree of cleanliness is required, decorative panels, sound diffusersFeatures: Kydex 115 meets the criteria for flame spread and smoke development that determines Class I/A compliance using ASTM E84 methodology. It is ideal for applications such as ceiling panels where the product must be routinely removed and/or cleaned for maintenance. It provides superior impact protection and well not chip, crack, or flake. Color is integral throughout each sheet. Kydex 115 has excellent chemical resistance allowing for the removal of tougher stains with stronger cleaning agents without damaging the surface of the sheet. This high rigidity fire rated sheet is a non-porous, tough, chemical resistant material. Clean Room Class 10 Federal Standard 209D.Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hrs @ 23°C
Water Absorption at Saturation 0.15 %
0.15 %
7 days at 23°C
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 39.6 MPa
5740 psi
ASTM D638
Modulus of Elasticity 2.392 GPa
346.9 ksi
Flexural Yield Strength 70.3 MPa
10200 psi
ASTM D790
Izod Impact, Notched 1.62 - 2.67 J/cm

@Temperature 23.0 °C
3.03 - 5.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
annealed; ASTM D648
Flammability Test 25
25
Flame Spread; All gauges from 0.028 in (0.71 mm) and greater. Not intended for specification purposes.; ASTM E84
440
440
Smoke Developed, Free Standing, Class 1/A