Kennametal Stellite Tribaloy® T-900

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Tribaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Tribaloy® T-900.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hardened by Laves phase, not by carbides. Higher ductility than Tribaloy® T-800.Applications: Used in applications with high temperatures and severe wear, abrasion, and corrosion.Corrosion: Good localized corrosion resistance.Weldability: Can be PTA welded with a preheat of 260°C (500°F) or higher.Wear: High temperature wear resistance. Wear test data: Method: block-on-ring; Block: alloy specimen; Ring: SAE 4620 steel, Rc 58-63, RMS 22-28 microns; Load: 90, 150, 210 lbs.; Sliding distance: 220 meters (2000 revolutions). Wear volume 90 lb. load: 0.000012(in^3), 150 lb. load: 0.000019(in^3), 210 lb. load: 0.000024(in^3); Mean wear scar width 90 lb. 0.07(in), 150 lb. 0.09(in), 210 lb. 0.09(in); Friction force 90 lb. 39(lb), 150 lb. 59(lb), 210 lb. 80(lb).Data provided by the manufacturer, Deloro Stellite, Inc.Product of former Deloro Stellite Inc.
Mechanical Properties Metric English Comments
Hardness, Brinell 476
476
Converted from Rockwell C hardness.
Hardness, Knoop 574
574
Converted from Rockwell C hardness.
Hardness, Rockwell A 75
75
Converted from Rockwell C hardness.
Hardness, Rockwell C 48 - 52
48 - 52
Retains hardness up to 2640°F (1450°C).
Hardness, Vickers 510
510
Converted from Rockwell C hardness.
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 18 %
18 %
Cobalt, Co 40.22 %
40.22 %
As remainder
Molybdenum, Mo 23 %
23 %
Nickel, Ni <= 16 %
<= 16 %
Silicon, Si 2.7 %
2.7 %