Material Notes:
Age-hardened, highly alloyed, nickel base alloy in the casting form. Hardened by the presence of intermetallic compounds in the highly alloyed matrix. Unique combination of corrosion and wear resistant.Applications: Used in high temperature, highly corrosive environments where good wear resistance in needed.Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Mechanical Properties Metric English Comments
Hardness, Brinell 383
383
Converted from Rockwell C hardness.
Hardness, Knoop 460
460
Converted from Rockwell C hardness.
Hardness, Rockwell A 71
71
Converted from Rockwell C hardness.
Hardness, Rockwell C 37 - 46
37 - 46
Hardness, Vickers 405
405
Converted from Rockwell C hardness.
Tensile Strength, Ultimate 600 MPa
87000 psi
Elongation at Break <= 1.0 %
<= 1.0 %
Compressive Yield Strength 1500 MPa
218000 psi
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 26 %
26 %
Iron, Fe <= 2.0 %
<= 2.0 %
Molybdenum, Mo 26 %
26 %
Nickel, Ni 44.5 %
44.5 %
As Remainder
Silicon, Si <= 1.5 %
<= 1.5 %