Kennametal Stellite Stellite® 12 PM cast

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Stellite® 12 PM cast.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: include vane plugs, fuel metering pins, spacer bushings, ball blanks (bearings), race blanks (bearings), diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts.Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.52 g/cc
0.308 lb/in³
theoretical
Mechanical Properties Metric English Comments
Hardness, Brinell 394
394
Converted from Rockwell C hardness.
Hardness, Knoop 473
473
Converted from Rockwell C hardness.
Hardness, Rockwell A 72
72
Converted from Rockwell C hardness.
Hardness, Rockwell B 113
113
Converted from Rockwell C hardness. Beyond normal Rockwell B range, for comparison only.
Hardness, Rockwell C 43
43
Hot hardness.
Hardness, Vickers 416
416
Converted from Rockwell C hardness.
Thermal Properties Metric English Comments
CTE, linear 11.9 µm/m-°C

@Temperature 0.000 - 100 °C
6.61 µin/in-°F

@Temperature 32.0 - 212 °F
12.8 µm/m-°C

@Temperature 0.000 - 200 °C
7.11 µin/in-°F

@Temperature 32.0 - 392 °F
12.9 µm/m-°C

@Temperature 0.000 - 300 °C
7.17 µin/in-°F

@Temperature 32.0 - 572 °F
13.4 µm/m-°C

@Temperature 0.000 - 400 °C
7.44 µin/in-°F

@Temperature 32.0 - 752 °F
13.8 µm/m-°C

@Temperature 0.000 - 500 °C
7.67 µin/in-°F

@Temperature 32.0 - 932 °F
14.1 µm/m-°C

@Temperature 0.000 - 600 °C
7.83 µin/in-°F

@Temperature 32.0 - 1110 °F
14.4 µm/m-°C

@Temperature 0.000 - 700 °C
8.00 µin/in-°F

@Temperature 32.0 - 1290 °F
15.2 µm/m-°C

@Temperature 0.000 - 800 °C
8.44 µin/in-°F

@Temperature 32.0 - 1470 °F
15.5 µm/m-°C

@Temperature 0.000 - 900 °C
8.61 µin/in-°F

@Temperature 32.0 - 1650 °F
15.8 µm/m-°C

@Temperature 0.000 - 1000 °C
8.78 µin/in-°F

@Temperature 32.0 - 1830 °F
Melting Point 1255 - 1341 °C
2291 - 2446 °F
Solidus 1255 °C
2291 °F
Liquidus 1341 °C
2446 °F
Component Elements Properties Metric English Comments
Boron, B 1.0 %
1.0 %
Carbon, C 1.5 %
1.5 %
Chromium, Cr 30 %
30 %
Cobalt, Co 48 %
48 %
As remainder
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni <= 3.0 %
<= 3.0 %
Other <= 3.0 %
<= 3.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 8.5 %
8.5 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 1.20

@Temperature 22.0 °C
<= 1.20

@Temperature 71.6 °F
200 Oersted