Kennametal Stellite Nistelle X Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Nistelle
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Nistelle X Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nistelle X possesses an exceptional combination of oxidation resistance, fabricability and high-temperature strength. It has been found to be exceptionally resistant to stress-corrosion cracking in petrochemical applications.Information provided by Kennametal Stelliteâ„¢
Component Elements Properties Metric English Comments
Carbon, C 0.15 %
0.15 %
Chromium, Cr 22 %
22 %
Cobalt, Co 1.5 %
1.5 %
Iron, Fe 18.5 %
18.5 %
Molybdenum, Mo 9.1 %
9.1 %
Nickel, Ni >= 45.75 %
>= 45.75 %
as balance
Other <= 1.0 %
<= 1.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition