Material Notes:
Nistelle C is designed primarily for high corrosion resistance, and therefore used for pumps and valve parts etc. in the chemical industry, and is available both for hardfacing by welding and as castings. Nistelle C has excellent high temperature strength and resistance to oxidation, being extensively used for hardfacing drop forging dies. It is readily machinable.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 17 - 27
17 - 27
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 17 %
17 %
Iron, Fe 6.0 %
6.0 %
Molybdenum, Mo 17 %
17 %
Nickel, Ni >= 54.1 %
>= 54.1 %
as balance
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 4.5 %
4.5 %
Vanadium, V 0.30 %
0.30 %
Descriptive Properties Value Comments
Application Technique HVOF & thermal spray
PTA & laser deposition