Kennametal Stellite Nistelle 718 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Nistelle
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Nistelle 718 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A precipitation-hardenable alloy. The alloy combines corrosion resistance and high strength with outstanding weldability including resistance to post weld cracking. The alloy has excellent creep-rupture strength at room temperatures to 1300ºF (700ºC). Applications include gas turbines, rocket motors, spacecraft, nuclear reactors, pumps and tooling.Information provided by Kennametal Stellite™
Mechanical Properties Metric English Comments
Hardness, Rockwell C <= 25
<= 25
Component Elements Properties Metric English Comments
Chromium, Cr 21.5 %
21.5 %
Cobalt, Co <= 2.0 %
<= 2.0 %
Iron, Fe 4.0 %
4.0 %
Molybdenum, Mo 13.5 %
13.5 %
Nickel, Ni >= 55.85 %
>= 55.85 %
as balance
Tungsten, W 3.0 %
3.0 %
Vanadium, V 0.15 %
0.15 %
Descriptive Properties Value Comments
Application Technique HVOF & thermal spray
PTA & laser deposition