Kennametal Stellite Hydroloy® HQ913®

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Kennametal Stellite
Trade Name Hydroloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Hydroloy® HQ913®.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Proprietary stainless steel with low Co and Mn contents, formulated to resist cavitation and droplet impingement erosion.Processing: Can be heat treated to increase ductility without affecting resistance to cavitation erosion. Work hardens easily; important to ensure good cutting action and to avoid rubbing during finishing operations. Easier to grind to final dimensions than the stainless steel it typically replaces.Corrosion Resistance: Moderate. Resists mildly corrosive environments and slight abrasive conditions.Applications: parts requiring cavitation or water droplet impingement erosion resistance such as hydraulic turbine runners or boiler feedwater pumps.Forms: Castings, wrought specialty shapes, hardfacing, wire, and powder.Product of former Deloro Stellite Inc. Similar to Ireca Alloy
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 274
274
Converted from Vickers hardness
Hardness, Knoop 306
306
Converted from Vickers hardness
Hardness, Rockwell C 32
32
Hardness, Vickers 290
290
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 448 MPa
65000 psi
Elongation at Break 35 %
35 %
Reduction of Area 40 %
40 %
Thermal Properties Metric English Comments
Melting Point 1400 - 1455 °C
2550 - 2651 °F
Solidus 1400 °C
2550 °F
Liquidus 1455 °C
2651 °F
Component Elements Properties Metric English Comments
Carbon, C 0.20 %
0.20 %
Chromium, Cr 17 %
17 %
Cobalt, Co 9.0 %
9.0 %
Iron, Fe 61.6 %
61.6 %
Manganese, Mn 9.5 %
9.5 %
Nitrogen, N 0.20 %
0.20 %
Silicon, Si 2.5 %
2.5 %