Material Notes:
Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal Stelliteâ„¢
Physical Properties Metric English Comments
Density 8.20 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 200
200
Tensile Strength, Ultimate 640 - 700 MPa
92800 - 102000 psi
Tensile Strength, Yield 360 - 480 MPa
52200 - 69600 psi
Proof Stress
Elongation at Break >= 13 %
>= 13 %
Flexural Modulus 170 GPa
24700 ksi
Thermal Properties Metric English Comments
CTE, linear 14.1 µm/m-°C

@Temperature 20.0 - 600 °C
7.83 µin/in-°F

@Temperature 68.0 - 1110 °F
Melting Point 1300 - 1370 °C
2370 - 2500 °F
Solidus 1260 - 1270 °C
2300 - 2320 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 24 %
24 %
Cobalt, Co <= 1.0 %
<= 1.0 %
Iron, Fe 1.0 %
1.0 %
Molybdenum, Mo 9.5 %
9.5 %
Nickel, Ni >= 60.95 %
>= 60.95 %
as balance
Niobium, Nb (Columbium, Cb) <= 1.0 %
<= 1.0 %
Other <= 0.50 %
<= 0.50 %
Silicon, Si <= 2.0 %
<= 2.0 %