Kennametal Stellite Delcrome 316L Iron Alloy

Category Metal , Ferrous Metal , Superalloy
Manufacturer Kennametal Stellite
Trade Name Delcrome
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Delcrome 316L Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Corrosion resistant alloys with moderate to high metal to metal wear resistance.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C >= 20
>= 20
Component Elements Properties Metric English Comments
Carbon, C <= 13 %
<= 13 %
Chromium, Cr 18 %
18 %
Iron, Fe >= 63.87 %
>= 63.87 %
as balance
Manganese, Mn 0.70 %
0.70 %
Molybdenum, Mo 2.6 %
2.6 %
Silicon, Si 1.8 %
1.8 %
Tungsten, W <= 0.030 %
<= 0.030 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition