Kazanorgsintez Synthanol DT-7

Category Fluid , Solvent
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez Synthanol DT-7.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Mixture of polyoxyethyleneglycol esters of synthetic primary alcohols of C10-C13 fractions. Application: Intended for use as an efficient nonionic surface-active substance.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
pH 7.5 - 11
7.5 - 11
pH value of water solution with 10% mass fraction
Descriptive Properties Value Comments
Appearance At 15°C to 25°C: Past-like syrupy mass of white slightly yellowish color
Cloud Point Temperature of Aqueous Solution with Mass Content of 1% (°C) 42-52