Material Notes:
Production Method: Ethylbenzene fraction is a by-product in the production of isopropyl benzene in the process of alkylation of benzene with propane-propylene fraction in the presence of aluminum chloride. Application: Ethylbenzene fraction is used as an ingredient in motor fuels.Information Provided by Kazanorgsintez
Thermal Properties Metric English Comments
Boiling Point <= 155 °C
<= 311 °F
Component Elements Properties Metric English Comments
Loss on Ignition(%) <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Appearance Colorless or slightly yellow liquid, free of mechanical impurities and water