Kazanorgsintez Aluminum Hydroxychloride

Category Ceramic , Halide
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez Aluminum Hydroxychloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Aluminum Hydroxychloride is a waste product of the process of benzene alkylation with olefin, obtained through washing out the reaction mass from complex catalyst with chloride aluminum solutions.Applications: Intended for use as a coagulant in the process of industrial wastewater purification and also as an agent for carbon deposits.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
pH 0.80 - 2.0
0.80 - 2.0
Activity index of hydrogen ions
Descriptive Properties Value Comments
Appearance Slightly yellow or gray color liquid with green tone
Mass concentration of basic material converted into AlCl3 (g/dm3) 200-300
Mass concentration of suspended particles (g/dm3) 0.5