Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and cable shielding by extrusion method.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.9185 - 0.924 g/cc
0.03318 - 0.0334 lb/in³
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
Melt Flow 0.21 - 0.39 g/10 min

@Load 21.6 kg
0.21 - 0.39 g/10 min

@Load 47.6 lb
±8%
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.80 MPa
>= 1420 psi
Elongation at Break >= 600 %
>= 600 %
Tear Strength Test >= 13.7
>= 13.7
MPa
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 200 °C

@Time >=900 sec
>= 392 °F

@Time >=0.250 hour
Electrical Properties Metric English Comments
Dielectric Constant <= 2.3

@Frequency 1000 Hz
<= 2.3

@Frequency 1000 Hz
Dielectric Strength >= 40.0 kV/mm

@Frequency 50.0 Hz
>= 1020 kV/in

@Frequency 50.0 Hz
Sample of 1 mm thickness, Alternating current
Dissipation Factor <= 0.00030

@Frequency 1000 Hz
<= 0.00030

@Frequency 1000 Hz
Descriptive Properties Value Comments
Amount of impurities [pcs] 15
Premium Quality
3
Superior Quality
Copyright © lookpolymers.com All Rights Reserved