Karina Karintox 70/6 Polyolefin Compound

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name Karintox
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina Karintox 70/6 Polyolefin Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Karintox is a thermoplastic polyolefin, flame retardant, non-halogen, and low smoke emission. Recommended for electrical coating for cables until 1KV. For a better usage/processing, manufacturer suggests a pre-warm/heat (2 hours in 70-80°C), mainly after being stocked for a long time. Low compression screws (1.2:1 is the ideal) and cleaving. Thermical profile from 140ºC to 165°C and melting temperatures no more than 180°C.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.45 g/cc
1.39 - 1.45 g/cc
ASTM D 792
Moisture Absorption <= 0.0600 %
<= 0.0600 %
ME-52
Deformation 30 %
30 %
Hot Deformation; NBR 6239
ASTM Color -1.28 - 1.72
-1.28 - 1.72
Color A, ME 12
1.77 - 4.77
1.77 - 4.77
Color B, ME 12
87.59 - 90.59
87.59 - 90.59
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 54

@Time 15.0 sec
50 - 54

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 10.0 MPa
>= 1450 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
>= 12.6 MPa
>= 1820 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 130 %
>= 130 %
After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
>= 150 %
>= 150 %
NBR NM-IEC 60811-1-1
Thermal Properties Metric English Comments
Brittleness Temperature <= -35.0 °C
<= -31.0 °F
ASTM D 746
Flammability Test 75
75
% Transmittance - Smoke Density Test; NBR 11300
Oxygen Index >= 36 %
>= 36 %
ASTM D 2863
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application 70 Grades
Bromine, Br (%) < 0.01
IEC 62321
Cold Blend OK
-15°C; NBR NM-IEC 60811-1-4
Corrosivity of Gases 5
Conductivity, mg/g (NBR 11633)
5,6.00
pH (NBR 11633)
Halogen Acid Gas Evolution (mg/g) 0
NBR 10495
Maximum Variation of Elongation (%) 20
NBR NM-IEC 60811-1-2
Maximum Variation of Tensile Strength (%) 20
NBR NM-IEC 60811-1-2
Toxicity Index 0,65.00
NBR 12139