Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E MCP 520 Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E MCP 520 Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -0.890 - 0.71
-0.890 - 0.71
Color A, ME 12
-0.860 - 0.74
-0.860 - 0.74
Color B, ME 12
27.17 - 28.77
27.17 - 28.77
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 14.7 MPa
>= 2130 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 270 %
>= 270 %
NBR NM-IEC 60811-1-1
Electrical Properties Metric English Comments
Volume Resistivity >= 3.00e+14 ohm-cm
>= 3.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application Drop Wire
Users viewing this material also viewed the following: