Karina E CAK 65 Ivory PVC Compound

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E CAK 65 Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reclaimed PVC compound, recommended for injection of footwear soles. Color it is not guaranteed. CAK = alternative compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.34 g/cc
1.28 - 1.34 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 5.88 MPa
>= 853 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 30.0 kN/m
>= 171 pli
DIN 53507
Abrasion <= 275
<= 275
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application General Purpose Soles
Users viewing this material also viewed the following: