Material Notes:
Crystal flexible PVC compound, recommended for extrusion of stretch films for general packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.31 g/cc
1.25 - 1.31 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 89

@Time 15.0 sec
85 - 89

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 14.7 MPa
>= 2130 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles
Clarity OK
ME 03
Users viewing this material also viewed the following: