Karina E 858-10/16-ERYA PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 858-10/16-ERYA PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
ASTM Color -3.99 - -0.990
-3.99 - -0.990
Color A, ME 12
6.1 - 9.1
6.1 - 9.1
Color B, ME 12
80.78 - 83.78
80.78 - 83.78
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Izod Impact, Notched >= 0.179 J/cm
>= 0.335 ft-lb/in
Method A; ASTM D 256
>= 0.583 J/cm
>= 1.09 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 72.8 °C
>= 163 °F
ASTM D 1525
Descriptive Properties Value Comments
Application General Purpose Profiles