Karina E 820-10/1-D-TR White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 820-10/1-D-TR White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.54 - 1.60 g/cc
1.54 - 1.60 g/cc
ASTM D 792
ASTM Color -1.73 - -0.130
-1.73 - -0.130
Color A, ME 12
4.28 - 5.88
4.28 - 5.88
Color B, ME 12
85.33 - 86.93
85.33 - 86.93
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application Sewer