Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.50 g/cc
1.44 - 1.50 g/cc
ASTM D 792
ASTM Color -2.65 - 0.35
-2.65 - 0.35
Color A, ME 12
2.28 - 5.28
2.28 - 5.28
Color B, ME 12
87.23 - 90.23
87.23 - 90.23
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 87

@Time 15.0 sec
83 - 87

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638