Karina E 72/206-IS Crystal PVC Compound (SP32811)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 72/206-IS Crystal PVC Compound (SP32811).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystal flexible PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.16 - 1.22 g/cc
1.16 - 1.22 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 74

@Time 15.0 sec
70 - 74

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 12.7 MPa
>= 1850 psi
ASTM D 638
Elongation at Break >= 260 %
>= 260 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles