Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 670D10/116-Y White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 670D10/116-Y White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.21 - 1.27 g/cc
1.21 - 1.27 g/cc
ASTM D 792
ASTM Color -1.96 - 1.04
-1.96 - 1.04
Color A, ME 12
-1.27 - 1.73
-1.27 - 1.73
Color B, ME 12
89.05 - 92.05
89.05 - 92.05
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 65 - 69

@Time 15.0 sec
65 - 69

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 30.0 kN/m
>= 171 pli
DIN 53507
Abrasion <= 180
<= 180
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts