Karina E 630-10/175-A-IS White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 630-10/175-A-IS White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
ASTM Color -2.53 - 0.47
-2.53 - 0.47
Color A, ME 12
-0.550 - 2.45
-0.550 - 2.45
Color B, ME 12
89.23 - 92.23
89.23 - 92.23
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 64

@Time 15.0 sec
60 - 64

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 12.7 MPa
>= 1850 psi
ASTM D 638
Elongation at Break >= 260 %
>= 260 %
ASTM D 638
Descriptive Properties Value Comments
Application Non Food