Karina E 48/1-FC-LMP Black Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 48/1-FC-LMP Black Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with inorganic pigments PVC resin based (carrier polymer) Supplied in pellet form and packaged in 25 KG bags Recommended use of 2% to 5%Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.19 - 1.23 g/cc
1.19 - 1.23 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -0.980 - 0.62
-0.980 - 0.62
Color B, ME 12
-0.840 - 0.76
-0.840 - 0.76
Color A, ME 12
27.3 - 28.9
27.3 - 28.9
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
NBR 7456
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application Extrusion
Injection
Bromine, Br (%) < 0.01
IEC 62321
RAL Classification (Natural Base) 9004