Karina E 45/56-GEN Gold MBATCH (SP31447) for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 45/56-GEN Gold MBATCH (SP31447) for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.48 - 1.54 g/cc
1.48 - 1.54 g/cc
ASTM D 792
ASTM Color 2.71 - 8.71
2.71 - 8.71
Color A, ME 12
20.63 - 26.63
20.63 - 26.63
Color B, ME 12
65.47 - 71.47
65.47 - 71.47
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 61 - 65

@Time 15.0 sec
61 - 65

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Extrusion