Karina E 42/234-FC-LMP MB Concentration de Pigment Red for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 42/234-FC-LMP MB Concentration de Pigment Red for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pigment Concentrate Recommended for Extrusion General PVC. Minimum usage 2%. Organic and Inorganic.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
NBR NM-IEC 60811-1-3
ASTM Color 19.85 - 22.85
19.85 - 22.85
Color B, ME 12
38.17 - 41.17
38.17 - 41.17
Color L, ME 12
40.32 - 43.32
40.32 - 43.32
Color A, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 74

@Time 15.0 sec
70 - 74

@Time 0.00417 hour
NBR 7456
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application Extrusion