Karina E 27/8-GIN Fume MBATCH (SP31452) for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 27/8-GIN Fume MBATCH (SP31452) for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recommended usage from 2% to 3% on crystal PVC compound (kind of gray for crystal)Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.19 - 1.25 g/cc
1.19 - 1.25 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Injection