Material Notes:
Recommended usage from 2% to 3% on crystal PVC compound (Gray to close the crystal). Close in this case means not clear/transparent.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Moisture Absorption <= 0.150 %
<= 0.150 %
ME-52
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Descriptive Properties Value Comments
Application Blow Molding
Extrusion
Injection
Bromine, Br (%) < 0.01
IEC 62321
Carrier Polymer EVA