Karina E 105908-35/1-C-IS-LMP Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 105908-35/1-C-IS-LMP Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC compound recommended for extrusion of wires TW and THW.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.29 - 1.35 g/cc
1.29 - 1.35 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 91

@Time 15.0 sec
87 - 91

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 12.7 MPa
>= 1850 psi
ASTM D 638
Elongation at Break >= 180 %
>= 180 %
ASTM D 638
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application 105 Grades
90 Grades