Material Notes:
Reclaimed PVC compound recommended for soles and general purpose injected articles (whose temperature of use do not exceed 40°C).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.25 - 1.35 g/cc
1.25 - 1.35 g/cc
ASTM D 792
ASTM Color -1.02 - 0.58
-1.02 - 0.58
ASTM B, ME 12
-0.720 - 0.88
-0.720 - 0.88
ASTM A, ME 12
25.1 - 26.7
25.1 - 26.7
ASTM L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 5307
Abrasion <= 300
<= 300
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.0 °C
104 °F
Descriptive Properties Value Comments
Application General Purpose Soles