Material Notes:
Reclaimed PVC compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.43 g/cc
1.37 - 1.43 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 33 - 37

@Time 15.0 sec
33 - 37

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 1.47 MPa
>= 213 psi
ASTM D 638
Elongation at Break >= 150 %
>= 150 %
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Soles