Karina BT-0002/17 White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina BT-0002/17 White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC compound with addition of nitrile rubber, recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.16 - 1.20 g/cc
1.16 - 1.20 g/cc
ASTM D 792
ASTM Color -2.06 - 0.94
-2.06 - 0.94
Color A, ME 12
1.71 - 4.71
1.71 - 4.71
Color B, ME 12
91.31 - 94.31
91.31 - 94.31
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 52

@Time 15.0 sec
48 - 52

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Tear Strength >= 18.0 kN/m
>= 103 pli
DIN 53507
Abrasion <= 250
<= 250
mm<sup>3</sup>; DIN 53516