Karina 846-32/64-IS-RG Orange PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 846-32/64-IS-RG Orange PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non toxic PVC compound, recommended for blow molded bottles for cosmetics packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.37 g/cc
1.31 - 1.37 g/cc
ASTM D 792
ASTM Color 28.81 - 30.41
28.81 - 30.41
Color B, ME 12
40.59 - 42.19
40.59 - 42.19
Color A, ME 12
60.36 - 61.96
60.36 - 61.96
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 34.3 MPa
>= 4980 psi
ASTM D 638
Descriptive Properties Value Comments
Application Cosmetics Packaging