Material Notes:
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM D 792
ASTM Color -1.49 - 0.51
-1.49 - 0.51
Color B, ME 12
-1.03 - 0.97
-1.03 - 0.97
Color A, ME 12
26.52 - 28.52
26.52 - 28.52
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 10.0 MPa
>= 1450 psi
ASTM D 638
>= 10.0 MPa
>= 1450 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
>= 200 %
>= 200 %
After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Coaxial