Karina 805-10/152-A-ERYB White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 805-10/152-A-ERYB White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.45 - 1.51 g/cc
1.45 - 1.51 g/cc
ASTM D 792
ASTM Color -1.74 - -0.140
-1.74 - -0.140
Color A, ME 12
2.77 - 4.37
2.77 - 4.37
Color B, ME 12
95.86 - 97.46
95.86 - 97.46
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Modulus of Elasticity >= 3.29 GPa
>= 477 ksi
ASTM D 638
Izod Impact, Notched >= 0.380 J/cm
>= 0.712 ft-lb/in
Method A; ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 80.0 °C
>= 176 °F
ASTM D 1525
Heat Distortion Temperature >= 76.0 °C
>= 169 °F
ASTM D 648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Application Automotive